1)Longer time Gas Nitriding treatment 2)special anti-wear & abrasion alloy (bimetallic) 3)tungsten carbide 4)cobalt base alloy 5)stainless steel 6)Gh113 nickel based alloy Treatment Nitriding treatment(>100 Hours) Depth of Nitrided Layer: 0.5-0.8 mm Hardness of Nitrided Layer: >950Hv Hard Chrome Plating treatment: Thickness of Hard Chrome Plating Layer: 0.03-0.08mm Hardness of Hard Chrome Plating Layer: ≥950HV Nickel alloy plating.treatment: Bimetallic Barrel Centrifugal Casting (Inlay Alloy) Bimetallic Screw: Plasma Alloy Coating Spraying Depth of Bimetallic Layer: >2mm Hardness of Bimetallic Layer: HRC55°-65° |